Knowledge base · Filament
Does PLA need drying?
Not always. Fresh PLA straight out of a vacuum-sealed bag usually prints well. Dry it when it shows signs of moisture, and store opened spools sealed so you need to dry it less often.
Signs PLA needs drying
Popping or hissing at the nozzle, extra stringing, rough or bubbly surfaces, or brittle filament that snaps on the spool. These can have other causes, so our sister site's is my filament wet? checklist helps you rule them out.
How it arrives
Many brands dry and vacuum-seal PLA before sale. Overture, for example, says on its listing that each spool is dried for 24 hours and vacuum-sealed.
Some materials need it far more
Nylon is much more demanding: Prusa recommends drying its PA11 at 90 °C for 6–8 hours if you are unsure how long the bag has been open.
Sources